MET GRCop-42 - technical data sheet
Copper alloys: MET GRCop-42Alternative designation: GRCop-42 / CuCrNb |
MET GRCop-42 is a dispersion strengthened copper alloy with high strength and a good resistivity against low cycle fatigue (LCF). With a conductivity reaching up to 75% of IACS, CuCrNb-alloys were originally designed for use in high heat flux applications, like for example in combustion chambers and nozzles, and therefore offer high oxidation resistance in harsh environment. |
Chemical composition |
Element | Min [wt%] | Max [wt%] |
Cr | 3,1 | 3,4* |
Nb | 2,7 | 3,0* |
O | - | 0,04 |
Al | - | 0,005 |
Fe | - | 0,005 |
Si | - | 0,005 |
Cu | Balance | Balance |
Particle Size Distribution (others on request) |
PSD range [µm] | d10min | d90max |
5 - 20 | 4 | 22 |
15 - 45 | 10 | 48 |
20 - 63 | 18 | 66 |
45 - 106 | 40 | 106 |
*Cr/Nb ratio of 1.12-1.15